Evolution Lite

Au (40.3%)-based dental metal-ceramic alloy, Type 4
Purchase Online Today

Evolution Lite is a reduced-gold ceramic alloy, suitable for conventional metal-ceramics. The higher strength imparts this alloy with a high marginal strength, in particular during multiple firing, and allows accurately fitting restorations to be produced.

Indications*

  • Onlays, ¾ crowns, crowns
  • Telescope crowns, conus crowns
  • Bridges
  • Wide-span bridges
  • Cast posts / cores, bars, attachments
  • Implant-supported superstructures
  • Partial dentures

Technical Data

Composition (%):  Au 40.3 | Pd 39.3 | Ag 9.2 | In 9.3 | Ga 1.8 | Ru <1.0
ISO  22674:2016
ADA Class: High Noble
Type / Color: 4 / White
Density (g/cm³) 12.8
Melting Range (Solidus/Liquidus): 1100 - 1260 °C
Elastic Modulus (GPa): 130
  Porcelain Fired        Hardened                  
Vickers Hardness: 280                           295
Tensile Strength (MPa): 790                           795
0.2% Proof Stress (MPa):  565                           650
Elongation (%): 12                              10

Advantages

  • Light oxide
  • Good melting and flow properties
  • High resistance to marginal deformation with multiple firings
  • Compatible with metal-ceramics (e.g. IPS Style)
  • Tested biocompatibility

Processing Data

Investment Material:  Phosphate-bonded
Preheating / Burn- out Temperature: 750 - 820 °C
Crucible  Ceramic crucible
Casting Temperature: 1315 - 1375 °C
Oxidation  °C/min/Vacuum: 950 / 5 / No
CTE: (25 – 500 °C): 14.2 x 10-6 /K
Recommended Metal Ceramic: IPS Style, IPS InLine One,  IPS InLine, IPS Classic
Laser Welding Wire: Laser Ceramic White

*See TYPE CLASSIFICATION DUE TO PHYSICAL PROPERTIES

Download Materials